Item | Testtoestand | Eenheid | 75% al2o3 | 90% al2o3 | 95% al2o3 | 99% al2o3 | 99.5% al2o3 | zirkonia | step |
Bulkdichtheid | g/cm3 | > 3.20 | > 3.40 | > 3.60 | 3.7 | 3.7 | 6 | ≥2.6 | |
Flexural -sterkte | N/m2×103 | 1.96 | 2.25 | 2.24 | > 2.24 | > 2.74 | 11 | 1.37 | |
Coëfficiënt van lineaire expansie | 20 ~ 800°C. | ×10-6/°C. | / | 6.3-7.3 | 6.5-8.0 | 6.5-8.0 | 6.5-8.0 | 9.5 | ≤8 |
Permitiviteit | 1 MHz | ≤9 | 8.5-9.5 | 9 tot 10 | 9-10.5 | 9-10.5 | / | ≤7.5 | |
10 GHz | / | / | 9 tot 10 | 9-10.5 | / | / | / | ||
Insertieverlies | 1 MHz | ×10-6 | ≤10 | ≤8 | ≤4 | ≤2.5 | ≤1.5 | / | ≤8.0 |
10 GHz | ×10-6 | / | / | ≤10 | ≤6 | / | / | / | |
Weerstand tegen bulkdichtheid | 100°C. | @cm | > 1012 | > 1013 | > 1013 | > 1013 | > 1014 | > 1012 | > 1012 |
Punctiesterkte | KV/mm | 20 | 15 | 15 | 15 | / | / | 20 | |
Warmtegeleiding | 20°C. | W/m@k | / | 16.8 | 25.2 | 25.2 | 29.2 | 3 | 2.9 |