Model | GW-TP-AJ | GW-TP-BJ | GW-AL | GW-BL | GW-CL | GW-DL | GW-EL | |
Hoofdcomponenten, % | (Al2O3+Cr2O3) ≥90 |
(Al2O3+Cr2O3) ≥90 |
(Al2O3+Cr2O3) ≥87 |
(Al2O3+Cr2O3) ≥85 |
(Al2O3+Cr2O3) ≥82 |
(Al2O3+Cr2O3) ≥80 |
(Al2O3+Cr2O3) ≥70 |
|
Koude verbrijzelingssterkte, MPa ≥ | 140 | 130 | 120 | 110 | 100 | 90 | 100 | |
Dichtheid, g/cm3 ≥ | 3.62 | 3.62 | 3.55-3.62 | 3.5-3.55 | 3.4-3.5 | 3.38-3.45 | 3.0-3.2 | |
Schijnbare porositeit, % ≤ | 10 | 10 | 10 | 14 | 15 | 16 | 20 | |
Brandwerendheid °C ≥ | 2050 | 2000 | 1850 | 1800 | 1800 | 1800 | 1810 | |
Thermische schokbestendigheid (1100°C waterkoeling), maal ≥ | 4 | 3 | 2 | 2 | 1 | 1 | 3 | |
Lineaire verandering naverwarming (1500°C x 3h), % | 0 | 0 | 0 | 0 | 0 | 0 | 0.1 | |
Refractoriteit onder belasting | °C ≥ | 1750 | 1750 | 1700 | 1700 | 1700 | 1700 | 1420 |
MPa x vervorming, % | 0.2 x 0.6 | 0.2 x 0.6 | 0.2 x 0.6 | 0.2 x 0.6 | 0.2 x 0.6 | 0.2 x 0.6 | 0.2 x 0.6 | |
De hardheid van MOH ≥ | 9 | 9 | 9 | 9 | 9 | 8.5 | 6.7 | |
Max. Bedrijfstemperatuur, °C ≥ | 1700 | 1700 | 1680 | 1680 | 1680 | 1680 | 1400 |