Type: | Alloy Steel Bar |
---|---|
Standaard: | AISI, ASTM, DIN, JIS |
Samenstelling: | Ferro Staalschroot |
Techniek: | Cold Drawn |
Vorm: | leiding |
Oppervlakte Behandeling: | Gepolijst |
Leveranciers met geverifieerde zakelijke licenties
Kwaliteit | C | SI | MN | P | S | CR | MA | V | Al |
37 Mn | 0.36-0.40 | 0.17-0.30 | 1.55-1.70 | Max 0.015 |
Max. 0.010 | Max0, 20 | Max0, 10 | Max. 0.05 | - |
37 Mn/1 | 0.36-0.40 | 0.17-0.30 | 1.55-1.70 | Max 0.015 |
Max. 0.010 | Max0, 20 | Max0, 10 | Max. 0.05 | 0.02- 0.045 |
37 Mn/2 | 0.34-0.38 | 0.17-0.30 | 1.50-1.70 | Max 0.015 |
Max. 0.010 | Max0, 20 | Max0, 10 | Max. 0.05 | |
34 Mn2V | 0.32-0.36 | 0.17-0.35 | 1.50-1.70 | Max 0.015 |
Max. 0.010 | Max0, 20 | Max0, 10 | 0.08-0.12 | - |
30CrMo | 0.28-0.32 | 0.17-0.35 | 0.45-0.65 | Max 0.015 |
Max. 0.010 | 0.90-1.1 | 0.18-0.25 | Max. 0.02 | 0.02-0.045 |
35CrMo | 0.33-0.39 | 0.17-0.35 | 0.45-0.65 | Max 0.015 |
Max. 0.010 | 0.90-1.1 | 0.18-0.25 | Max. 0.05 | - |
34CrMo4 | 0.30-0.35 | 0.17-0.35 | 0.65-0.80 | Max 0.015 |
Max. 0.010 | 0.90-1.1 | 0.18-0.25 | Max. 0.05 | 0.02-0.045 |
Als< 0.02%, Sn< 0.02%, AS+Sn+SB+PB+Bi< 0.035, V+NB+Ti+B+ZR< 15% |
Kwaliteit | Verwarmingstemperatuur (ºC) | Koelweg | Treksterkte (MPa) | Opbrengststerkte (MPa) | Verlenging | Impact waarde |
37 Mn | 820-860 afdrenken 550-650 temperen |
water | > =750 | > =630 | > =16 | > =27(-50ºC) |
37 Mn/1 | 820-860 afdrenken 550-650 temperen |
water | > =750 | > =630 | > =16 | > =30(-50ºC) |
37 Mn/2 | 820-860 afdrenken 550-650 temperen |
water | > =750 | > =630 | > =16 | > =30(-50ºC) |
34 Mn2V | 820-860 afdrenken 550-650 temperen |
water | > =745 | > =530 | > =16 | > =27(-50ºC) |
30CrMo | 820-860 afdrenken 550-650 temperen |
water | > =930 | > =785 | > =12 | > =27(-50ºC) |
35CrMo | 820-860 afdrenken 550-650 temperen |
water | > =980 | > =835 | > =12 | > =27(-50ºC) |
34CrMo4 | 820-860 afdrenken 550-650 temperen |
water | > =950 | > =850 | > =14 | > =30(-50ºC) |