Gegalvaniseerde staaldraad ASTM- A641/ A641M-03-warm gegalvaniseerde draad PARAMETERS:
LAAG KOOLSTOFGEHALTE |
MEDIUM KOOLSTOF |
HOGE KOOLSTOFUITSTOOT |
FORMAAT/ mm |
ZINKCOATING-g/m2 |
TOLERANTIE/ mm |
TREKSTERKTE |
KLASSE A Min. |
KLASSE 4 min. |
0.90 |
137 |
- |
±0.05 |
INDIEN NODIG |
1.00 |
153 |
- |
1.20 |
168 |
- |
1.40 |
183 |
- |
1.60 |
198 |
- |
1.80 |
198 |
- |
1.90 |
214 |
- |
2.00 |
214 |
366 |
±0.10 |
2.30 |
229 |
366 |
2.50 |
244 |
366 |
2.70 |
244 |
366 |
3.00 |
259 |
366 |
3.40 |
259 |
366 |
3.80 |
275 |
366 |
±0.10 |
4.10 |
275 |
366 |
4.50 |
275 |
366 |
4.90 |
305 |
366 |
5.30 |
305 |
366 |
Groter naar behoefte |
|
Tot 450 g/m2 |
±0.13 |
|
|
|
|
|
|
Zink-5% aluminium-gemengd mischmetaal staaldraad met een legering CHEMISCH COMPOSITON %
Al |
CE+La |
FE |
SI |
PB |
CD |
SN |
4.20-6.20 |
0.03-0.10 |
Max. 0.075 |
Max. 0.015 |
Max. 0.005 |
Max. 0.05 |
Max. 0.005 |
COMMON-TENSIELE KWALITEIT / PARAMETERS:
FORMAAT/mm |
ZINKCOATING- g/m2 |
TREKSTERKTE/MPA |
1% ENLONGATION MPA≥ |
L0=250mm / % ENLONGATIE/ ≥ |
KLASSE A |
KLASSE B |
1.24-2.25 |
185-215 |
1340 |
1240 |
1170 |
1100 |
3.0-3.5 |
2.25-2.75 |
215-230 |
1310 |
1210 |
1140 |
1070 |
3.0-3.5 |
2.75-3.00 |
245-260 |
1310 |
1210 |
1140 |
1070 |
3.0-3.5 |
3.00-3.50 |
245-260 |
1290 |
1190 |
1100 |
1000 |
3.0-3.5 |
3.50-4.25 |
260-275 |
1290 |
1190 |
1100 |
1000 |
4.0 |
4.25-4.75 |
260-275 |
1290 |
1190 |
1100 |
1000 |
4.0 |
4.75-5.50 |
290 |
1290 |
1190 |
1100 |
1000 |
4.0 |
HOGE TREKSTERKTE / PARAMETERS:
FORMAAT/mm |
ZINKCOATING- g/m2 |
TREKSTERKTE/MPA |
1% ENLONGATION MPA≥ |
L0=250mm / % ENLONGATIE/ ≥ |
KLASSE A |
KLASSE B |
1.24-2.25 |
185-215 |
1450 |
1380 |
1310 |
1240 |
2.5 |
2.25-2.75 |
215-230 |
1410 |
1340 |
1280 |
1210 |
2.5 |
2.75-3.00 |
245-260 |
1410 |
1340 |
1280 |
1210 |
3.0 |
3.00-3.50 |
245-260 |
1410 |
1340 |
1240 |
1170 |
3.0 |
3.50-4.25 |
260-275 |
1380 |
1280 |
1170 |
1100 |
3.0 |
4.25-4.75 |
260-275 |
1380 |
1280 |
1170 |
1100 |
3.0 |
4.75-5.50 |
290 |
1380 |
1280 |
1170 |
1100 |
3.0 |
Warm gegalvaniseerde staalkerndraad met een hoog koolstofgehalte voor de 'ACSR'-kabel ASTM B498 (BS4565-90 EN IEC60-888) CHEMISCH COMPOSITON %
C |
SI |
MN |
P |
S |
0.50-0.85 |
0.10-0.35 |
0.50-1.10 |
Max. 0.035 |
Max. 0.045 |
PARAMETERS:
FORMAAT/ mm |
Min. ULTIEME TREKSTERKTE/MPA |
TOLERANTIE/ mm |
ENLONGATIE in 250mm % |
ZINKCOATING- g/m2 |
KLASSE A |
KLASSE B |
KLASSE C |
1.60-2.30 |
1450 |
1380 |
1310 |
+0.04 -0,03 |
3.0-4.0 |
210 |
420 |
- |
2.30-3.05 |
1410 |
1340 |
1280 |
±0.05 |
240 |
480 |
- |
3.05-3.60 |
1410 |
1340 |
1280 |
+0,08 -0,05 |
260 |
520 |
- |
3.60-4.80 |
1380 |
1280 |
1240 |
+0,10 -0,08 |
300 |
- |
- |